Used steels:
Low-medium and high carbon content steels are
used, bought from leading European manufacturers
according to our specifications.
Steels which are generally used are:
CB4FF -19MNB4 - 30MNB3 - C35 BORO - 34Cr4 -
41 Cr4 - 38NICrMO4 - 42NICrMO4
|
|
Surface treatment leading to total or partial
hardening:
casehardening – carbonitriding – nitrating induction hardening
|
|
Surface protection treatment:
Electrolytic galvanising without Cr6 in the different thicknesses
Dacromet 320A - 320B - 500A - 500B
Geomet 321A-B
Geomet 500A - B
Geomet Plus
Deltatone/Deltaseal
Delta Protekt kl 100
Delta Protekt VH 301 GZ
Zintek 200 - Zintek/Techseal - ZintekTop
Phosphatising – Phosphatising + oiling
Hot deep Galvanizing |
|
 |
 |
 |
 |
|
|
|
|
 |
|
 |
 |
|
Cold Forging Division:
Production through a cold forging technique of products
in steel, starting from ø6 to ø33, in proportional lengths
to the ø from l = 10 mm to l = 240 mm
|
|
Hot Forging Division:
Production through a hot forging technique
followed by mechanical turning, milling, drilling,
grinding, on of special parts, from ø min. 10 mm. to
max ø 100 mm, in lengths from min. 10 mm
to max 2,000 mm., whose weight go
from min 50 gr. to max 25 kg.
|
|
Resistance classes:
4.6 - 5.6 - 8.8 - 9.8 - 10.9 - 12.9 - B7 - B7M
|
 |
|
 |
 |
 |
 |
|
|
|
|